Diameters / Packaging
Diameters |
1 ea Box |
1 ea Tube |
10 kg Tube/Box |
---|---|---|---|
0.094 in (2.4 mm) | ZN78CW09420POP | ||
2mm | ZN98CW20500L | ||
2mm X 500mm | ZN98CW20500 |
DETAILS
Aluxcor® zinc-aluminum flux-cored brazing alloy is designed for low temperature joining of aluminum base metals. Typical aluminum brazing alloys melt and flow very close to the base metal melting temperature. The zinc-aluminum alloy's lower operating temperatures reduce the possibility of overheating the aluminum part. Typical applications include joining aluminum alloys of the 1000, 3000 and 6000 series and joining aluminum-to-copper.
Features
- Aluxcor® zinc-aluminum alloys contain a cesium-fluoroaluminate (CsAlF) type flux in an internal core.
- The core percentage and dimensions are calculated to deliver optimum flux release and braze joint protection during heating.
- Post braze residue from this flux is non-corrosive, so removal is typically unnecessary.
- Flux inner core means no manual flux application is required, providing significant cost savings
- Melting range of 710°F - 898°F (377°C - 481°C).
- Recommended joint clearance is 0.003 - 0.005 in. (0.076 - 0.127 mm)
- Typical applications include brazing aluminum alloys of the 1000, 3000 and 6000 series and joining aluminum-to-copper.
- For dissimilar metal applications, consider the long-term galvanic corrosion potential as it may require a protective joint coating.
- Complies with the EU Reach & RoHS directive.
Typical Applications
- Joining aluminum alloys of 1000, 3000 and 6000 series
- Joining aluminum-to-copper