AZ91A magnesium TIG (GTAW) welding rod for joining with similar AZ91A filler metals, cast to wrought and wrought alloys. Magnesium rapidly oxidizes when melted, so proper shielding gas coverage is important. Always clean surfaces and edges adjacent to the weld prior to welding. Conforms to AWS A5.19 and AWS A5.8 (BMg-1) specifications.
Características
- Magnesium AZ92A TIG (GTAW) welding alloy
- For joining AZ92A to similar filler metals and wrought alloys
- Rigidly controlled manufacturing to conform to AWS A5.19, ER AZ92A and AWS A5.8 (BMg-1)
- Proper shielding is required to avoid oxidation
Aplicaciones Típicas
- Joining similar AZ92A filler metals
- Cast to wrought
- Wrought alloys
Posiciones de soldadura
- All